Hydrofluoric acid concentration, time and use of phosphoric acid on the bond strength of feldspathic ceramics

Abstract The objective of this study was to evaluate the influence of hydrofluoric acid (HF) concentration, etching time, and application of phosphoric acid (PA) followed by neutralization with sodium bicarbonate on the bond strength between a feldspar ceramic and resin cement. Thus, 80 blocks (10 x 12 x...

Effect of hydrofluoric acid concentration and etching time on resin-bond strength to different glass ceramics

Abstract: The objective of this study was to evaluate the effect of the hydrofluoridric acid (HF) concentration and time of acid conditioning on bond strength of three glass ceramics to a resin cement. Thus, fifty blocks (10 mm x 5 mm x 2 mm) of each ceramic (LDCAD: IPS e.max CAD; LCAD: IPS Empress CAD a...

Adhesion to a lithium disilicate glass ceramic etched with hydrofluoric acid at distinct concentrations

Braz. dent. j; 29 (5), 2018
Abstract This study evaluated the effect of different hydrofluoric acid (HF) concentrations on the bond strength between a lithium disilicate-based glass ceramic and a resin cement. Eighty ceramic-blocks (12×7×2 mm) of IPS e.Max CAD (Ivoclar Vivadent) were produced and randomly assigned to 8 groups, co...

The effect of hydrofluoric acid and resin cement formulation on the bond strength to lithium disilicate ceramic

Abstract To investigate how the hydrofluoric acid (HF) concentrations applied to a lithium disilicate glass-ceramic (EMX) affects the surface morphology and microtensile bond strength (μTBS) of ceramics to dentin, using light-cured resin cements with or without UDMA. Sixty-three EMX square ceramic b...

Micromorfología superficial de 2 cerámicas grabables tratadas con diferentes ácidos

Para lograr una unión fuerte entre las restauraciones de cerámica sin metal y las resinas de cementación se indican acondicionamientos de superficie previos a la cementación. Nuestro objetivo es describir y comparar al MEB las superficies de cerámicas feldespáticas y reforzadas con disilicato de li...

Influência do tempo de condicionamento ácido na alteração superficial, resistência de união e compressão da cerâmica de dissilicato de lítio

Este estudo in vitro propôs analisar os padrões de condicionamento da superfície da cerâmica a base de dissilicato de lítio após três tempos de condicionamento com ácido fluorídrico a 10%, a influência desses tempos na resistência ao cisalhamento de cilindros cerâmicos e à compressão...

Four chemical methods of porcelain conditioning and their influence over bond strength and surface integrity

OBJECTIVE: To assess four different chemical surface conditioning methods for ceramic material before bracket bonding, and their impact on shear bond strength and surface integrity at debonding.METHODS: Four experimental groups (n = 13) were set up according to the ceramic conditioning method: G1 = 37% p...